Technical data
| Items | Index |
| Appearance | White or light yellow powder |
| Stacking density, g/cm3 | 0.80±0.20 |
| Water solubility,% | 100 |
| Moisture,% | ≤5.0 |
Property of cement slurry
| Items | Index | Test Condition |
| Water loss, mL | ≤50 | 52℃,6.9MPa |
| Thickening time, min | ≥60 |
52℃,35.6MPa/26min |
| Initial consistency, Bc | ≤25 | |
| Compressive strength,
MPa |
≥14 |
52℃,Atmospheric pressure, 24h |
| Free water, mL | ≤1.0 | 52℃,Atmospheric pressure |
| The cement paste consists of 100% G grade cement (high sulfur resistance), +47.0% mixed water +0.6% OOC-G87S-A+0.5% OOC-X60L. | ||